Injection Molding
1 visualizações
Severe EAA internal stress concentration
Fenómeno do problema
EAA products with internal stress >15MPa causing cracking during storage
Análise das causas
Injection speed too fast causing large orientation stress; uneven cooling freezing in thermal stress; improper gate position causing concentrated flow orientation
Solução
1) Reduce injection speed to reduce orientation; 2) Uniform mold temperature to reduce thermal stress; 3) Anneal at 80°C/4h to release stress; 4) Optimize gate position
Conclusão principal
Internal stress is caused by fast injection and uneven cooling; reducing speed, uniform cooling and annealing are key