Extrusion & Post 13 visualizações

EEA extruded film has gel particles

Fenómeno do problema
Transparent gel particles of 0.1-0.5mm appearing on the EEA extruded film surface
Análise das causas
High molecular weight components in EEA not fully melted during extrusion forming local high crystallization zones; extrusion temperature too low or insufficient mixing
Solução
1) Increase extrusion temperature by 5-10°C to ensure full melting; 2) Increase screw mixing section length; 3) Inspect raw material to ensure consistent grade; 4) Replace with a finer 120-mesh screen to intercept unmelted particles
Conclusão principal
Gel particles are caused by insufficient melting; increasing temperature and mixing is the key
EEA filmgel particlesmelting temperaturemixing sectionhigh molecular weight components