Injection Molding 1 visualizações

EEA Severe Internal Stress Concentration

Fenómeno do problema
EEA product internal stress >15MPa causes cracking during storage
Análise das causas
Injection speed too fast, large orientation stress; uneven cooling freezes thermal stress; improper gate position, concentrated flow orientation
Solução
1) Reduce injection speed to reduce orientation; 2) Uniform mold temperature to reduce thermal stress; 3) Anneal at 80°C/4h to release stress; 4) Optimize gate position
Conclusão principal
Internal stress is caused by fast injection and uneven cooling; reducing speed, uniform cooling and annealing are key
EEA internal stress orientation stress annealing treatment uniform cooling