EEA Severe Internal Stress Concentration

Problem Phenomenon
EEA product internal stress >15MPa causes cracking during storage
Cause Analysis
Injection speed too fast, large orientation stress; uneven cooling freezes thermal stress; improper gate position, concentrated flow orientation
Solution
1) Reduce injection speed to reduce orientation; 2) Uniform mold temperature to reduce thermal stress; 3) Anneal at 80°C/4h to release stress; 4) Optimize gate position
Key Takeaway
Internal stress is caused by fast injection and uneven cooling; reducing speed, uniform cooling and annealing are key