Extrusion & Post
13 visualizações
Longitudinal Stripes on PU Extruded Film
Fenómeno do problema
Continuous stripes 1-3mm wide along the extrusion direction on PU extruded film surface
Análise das causas
Die lip local damage or gap uneven; melt stagnation zone in the die producing unstable flow; pressure fluctuation at the screw front
Solução
1) Check die lip flatness and gap uniformity ±0.01mm; 2) Clean the die interior to remove stagnation zone carbides; 3) Install a gear pump on the extruder to stabilize melt pressure; 4) Polish die lip to Ra<0.1μm
Conclusão principal
Longitudinal stripes are caused by die defects and pressure fluctuation; die maintenance and pressure stabilization are key
Isto foi útil?
0 pessoas acharam isto útil