Glass Fibre internal shrinkage void
Fenómeno do problema
Glass Fibre thick-wall product center shrinkage void diameter 0.5-2mm
Análise das causas
Thick-wall region after cooling interior shrinks but surface already solidified, cannot feed; holding time insufficient, gate freezes too early
Solução
1) Extend holding time until gate completely frozen; 2) increase gate size to delay freezing; 3) product design reduces wall thickness difference
Conclusão principal
Shrinkage void is caused by thick-wall shrinkage and insufficient holding; extending holding is key