Molds & Tooling 5 görüntüleme

Glass Fibre internal shrinkage void

Sorun Belirtisi
Glass Fibre thick-wall product center shrinkage void diameter 0.5-2mm
Neden Analizi
Thick-wall region after cooling interior shrinks but surface already solidified, cannot feed; holding time insufficient, gate freezes too early
Çözüm
1) Extend holding time until gate completely frozen; 2) increase gate size to delay freezing; 3) product design reduces wall thickness difference
Temel Çıkarım
Shrinkage void is caused by thick-wall shrinkage and insufficient holding; extending holding is key
Glass Fibreshrinkage voidthick wallholding timegate freezing