Blow Molding 7 visualizações

MP extrusion '2079851475616104457 severe parison sag

Fenómeno do problema
MP extrusion '2079851475616104457 parison sag 20-40mm causes bottle bottom wall thickness of only 0.3-0.4mm
Análise das causas
MP melt strength low, parison stretched thinner under gravity; parison extrusion speed slow, increasing sag time; parison temperature high, viscosity low, aggravating sag
Solução
1) add slight crosslinking agent 0.3-0.5wt% to increase melt strength; 2) increase parison extrusion speed to shorten sag time; 3) reduce parison temperature 10-15°C to increase viscosity; 4) wall thickness controller to compensate sag
Conclusão principal
parison sag is caused by low melt strength; slight crosslinking and wall thickness control are key
MP '2079851475616104457 parison sag melt strength slight crosslinking wall thickness control