ECTFE '2079851475616104452 cycle too long affects efficiency
Fenómeno do problema
2079851475616104452 cycle exceeds the target by more than 20%
Análise das causas
Cooling time accounts for a large proportion, insufficient plasticization, slow mold opening and closing
Solução
Optimize cooling water channels, increase plasticizing capacity, speed up mold opening and closing
Conclusão principal
Cycle optimization is the key to increasing production and reducing cost