Injection Molding 2 views

ECTFE '2079851475616104452 cycle too long affects efficiency

Problem Phenomenon
2079851475616104452 cycle exceeds the target by more than 20%
Cause Analysis
Cooling time accounts for a large proportion, insufficient plasticization, slow mold opening and closing
Solution
Optimize cooling water channels, increase plasticizing capacity, speed up mold opening and closing
Key Takeaway
Cycle optimization is the key to increasing production and reducing cost
ECTFEmolding cycle