Molding Process
8 visualizações
Circumferential cracks in welds
Fenómeno do problema
Circumferential cracks in hot-melt welds and low pressure bearing
Análise das causas
The heating time is short and melting is insufficient; the pressure is large and the weld is thin
Solução
Extend the heating time, reduce the pressure to 0.15MPa, heat preservation, NDT testing
Conclusão principal
Circumferential cracks are a major hidden danger of welds
Isto foi útil?
0 pessoas acharam isto útil