Molding Process
4 visualizaciones
Circumferential cracks in welds
Fenómeno del problema
Circumferential cracks in hot-melt welds and low pressure bearing
Análisis de la causa
The heating time is short and melting is insufficient; the pressure is large and the weld is thin
Solución
Extend the heating time, reduce the pressure to 0.15MPa, heat preservation, NDT testing
Conclusión clave
Circumferential cracks are a major hidden danger of welds
¿Le ha resultado útil?
0 personas encontraron esto útil