Extrusion & Post
7 visualizações
Metallocene linear low density polyethylene film cooling line height instability
Fenómeno do problema
The cooling line (frost line) height of the blown film fluctuates greatly, and film thickness and quality are unstable.
The cooling line height reflects the stability of cooling conditions and directly affects film performance.
Análise das causas
(1) Air ring air volume or air speed unstable\
(2) Extrusion temperature fluctuates\
(3) Ambient airflow interference\
(4) Screw speed fluctuates\
(5) Cooling air temperature fluctuates
Solução
(1) Check the air ring fan and valves, ensure stable air volume\
(2) Stabilize the extrusion temperature, fluctuation controlled within ±3°C (190-260°C range)\
(3) Install wind shields or isolation curtains to reduce ambient airflow interference\
(4) Stabilize the screw speed\
(5) Use constant-temperature cooling air to reduce temperature fluctuations
Conclusão principal
Cooling line instability is caused by fluctuations in cooling or extrusion conditions, requiring stabilization of air ring parameters and environmental conditions.
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!