Extrusion & Post
8 visualizaciones
Metallocene linear low density polyethylene film cooling line height instability
Fenómeno del problema
The cooling line (frost line) height of the blown film fluctuates greatly, and film thickness and quality are unstable.
The cooling line height reflects the stability of cooling conditions and directly affects film performance.
Análisis de la causa
(1) Air ring air volume or air speed unstable\
(2) Extrusion temperature fluctuates\
(3) Ambient airflow interference\
(4) Screw speed fluctuates\
(5) Cooling air temperature fluctuates
Solución
(1) Check the air ring fan and valves, ensure stable air volume\
(2) Stabilize the extrusion temperature, fluctuation controlled within ±3°C (190-260°C range)\
(3) Install wind shields or isolation curtains to reduce ambient airflow interference\
(4) Stabilize the screw speed\
(5) Use constant-temperature cooling air to reduce temperature fluctuations