7 visualizações
PET preforms turn yellow during storage
Fenómeno do problema
PET preforms turn yellow after 3-6 months of warehouse storage and cannot be used for transparent bottles.
Análise das causas
The thermal history and residual stress from preform processing are slowly released during storage; oxidative degradation continues to occur; storage temperature is on the high side.
Solução
Reduce preform processing temperature; store at ≤25°C away from light; manage on a first-in, first-out basis; seal preform packaging to prevent oxidation.
Conclusão principal
PET preform quality management during storage is an important link in the supply chain.