Injection Molding
7 visualizações
PETG injection molded part shrinkage rate too large
Fenómeno do problema
The shrinkage rate of PETG injection molded products exceeds 0.5%, and the dimensions deviate from the mold design.
Análise das causas
Holding pressure and holding time insufficient, feeding inadequate, mold temperature high with large cooling shrinkage, processing temperature high with large specific volume.
Solução
Increase holding pressure (60-70% of injection pressure) and extend holding time; appropriately lower the mold temperature to 20-40°C; control melt temperature at 230-250°C.
Conclusão principal
PETG is an amorphous material, and the shrinkage rate is mainly controlled by holding pressure and cooling.