Injection Molding 5 visualizações

PETG '2079851475616104452 poor thermal stability, residence time sensitive

Fenómeno do problema
When staying at high temperature for a long time, the melt color deepens and viscosity decreases, and product quality deteriorates.
Análise das causas
PETG has limited thermal stability at high temperature and undergoes thermal degradation during long residence.
Solução
Shorten the molding cycle and residence time; lower the rear barrel section temperature; avoid production interruptions; lower the temperature before shutdown.
Conclusão principal
PETG thermal stability needs to be maintained in continuous stable production.
PETGthermal stabilityresidence timedegradation

Isto foi útil?

0 pessoas acharam isto útil