Injection Molding 2 views

PETG '2079851475616104452 poor thermal stability, residence time sensitive

Problem Phenomenon
When staying at high temperature for a long time, the melt color deepens and viscosity decreases, and product quality deteriorates.
Cause Analysis
PETG has limited thermal stability at high temperature and undergoes thermal degradation during long residence.
Solution
Shorten the molding cycle and residence time; lower the rear barrel section temperature; avoid production interruptions; lower the temperature before shutdown.
Key Takeaway
PETG thermal stability needs to be maintained in continuous stable production.
PETGthermal stabilityresidence timedegradation