Molds & Tooling 7 visualizações

Center porosity of large parts

Fenómeno do problema
Micro shrinkage cavities or porosity appear in the center area of large thick-walled parts
Análise das causas
The shrinkage compensation distance exceeds the material's capability, causing insufficient compensation at the far end; holding pressure attenuates along long flow paths; gate position and number are improper
Solução
Increase the number of gates to shorten the shrinkage compensation distance; use sequential valve gates for staged compensation; increase holding pressure to compensate for pressure attenuation
Conclusão principal
Gate layout and sequential injection design of large parts are the key to success