Molds & Tooling 8 visualizaciones

Center porosity of large parts

Fenómeno del problema
Micro shrinkage cavities or porosity appear in the center area of large thick-walled parts
Análisis de la causa
The shrinkage compensation distance exceeds the material's capability, causing insufficient compensation at the far end; holding pressure attenuates along long flow paths; gate position and number are improper
Solución
Increase the number of gates to shorten the shrinkage compensation distance; use sequential valve gates for staged compensation; increase holding pressure to compensate for pressure attenuation
Conclusión clave
Gate layout and sequential injection design of large parts are the key to success
porositylarge partsshrinkage compensation distancesequential valvegate layout