Molds & Tooling 7 visualizações

High fiber content product filling difficulty

Fenómeno do problema
LGFPP with fiber content >40% has extremely poor flowability, and thin-wall products cannot be filled completely
Análise das causas
Fibers form a physical network structure restricting PP molecular chain movement; friction resistance between fibers greatly increases the apparent viscosity of the system; fibers hinder melt flow in the cavity
Solução
Appropriately increase the processing temperature to improve flowability (not exceeding the degradation temperature of 240°C); add processing aids to reduce inter-fiber friction; reduce fiber content to 30-35% or shorten fiber length
Conclusão principal
Fiber content and processing flowability conflict with each other within a certain range and need to be balanced
filling difficultyfiber contentnetwork structureprocessing aidflowability

Isto foi útil?

0 pessoas acharam isto útil