Respostas práticas para os desafios comuns dos materiais plásticos

11636 perguntas
Q
Ovality of linear low-density polyethylene pipes exceeding standard
Q
Mechanical properties of linear low-density polyethylene extruded products not meeting standards
Q
Excessive gel/gel particles in linear low-density polyethylene extruded products
Q
Bending deformation of linear low-density polyethylene extruded pipes
A
Pipe bending is caused by non-uniform cooling or haul-off eccentricity and needs to be solved from cooling uniformity and equipment alignment.
Extrusion & Post pipe bendinguneven coolinghaul-off alignmentuniform wall thicknessstraightness
Q
Uneven thickness of linear low-density polyethylene cast film
Q
Wrinkles appearing in linear low-density polyethylene blown film
Q
Die marks/lines appearing on linear low-density polyethylene extruded products
A
Die marks are caused by die inner wall damage or impurities; the die condition needs to be regularly cleaned and inspected.
Extrusion & Post die marksdie scratchesimpurity cleaningflow channel designscreen
Q
Insufficient equipment maintenance during linear low-density polyethylene linear low-density polyethylene processing
A
Equipment maintenance is the foundation of stable production; a standardized regular maintenance system and record system need to be established.
Molds & Tooling equipment maintenancepreventive maintenancescrew clearancemold maintenancesensor calibration
Q
Uneven thickness of linear low-density polyethylene blown film
A
Uneven film thickness is caused by uneven die gap, temperature or cooling and needs to be solved from mold precision and process stability.
Extrusion & Post film thicknessdie gaptemperature uniformityair ring coolinghaul-off stability
Q
Large current fluctuation of linear low-density polyethylene extruder
A