Material Drying 5 görüntüleme

ASA moisture content target management

Sorun Belirtisi
[Problem phenomenon] ASA drying released based on time, moisture content fluctuates greatly, product appearance varies between good and bad
Neden Analizi
Moisture content target is about below 0.05%, which cannot be guaranteed by drying time alone: environmental humidity, material layer thickness, dryer performance differences all affect the endpoint; moisture meter measurement is the release basis
Çözüm
Equip a moisture analyzer for batch sampling; release when moisture content ≤0.05%; drying parameters fine-tuned with seasonal humidity and recorded; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Temel Çıkarım
ASA drying looks at moisture content not the clock, only release below 0.05%; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
moisture contentdryingmoisture meterrelease

Bu faydalı oldu mu?

0 kişi bunu faydalı buldu

ChemAI