Molds & Tooling
4 görüntüleme
PCABS mold temperature and internal stress
Sorun Belirtisi
【Problem Phenomenon】PC/ABS mold temperature too low, parts have large internal stress, high risk of cracking and warpage
Neden Analizi
Mold temperature 60-80℃ recommended: high mold temperature 80℃ improves surface and reduces internal stress; low mold temperature 60℃ shortens the cycle but increases warpage risk; the PC component is sensitive to stress
Çözüm
For appearance and stress-sensitive parts, take mold temperature 75-80℃; for cycle-priority parts, 60-70℃; uniformize cavity temperature difference; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
PC/ABS mold temperature 60-80℃, stress parts take the upper limit; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu