Injection Molding
7 görüntüleme
PC holding pressure and sink mark stress
Sorun Belirtisi
【Problem Phenomenon】PC holding pressure improper, sink marks and internal stress problems alternate
Neden Analizi
PC shrinkage rate 0.5-0.7% is small but holding pressure shrinkage compensation is still needed; holding pressure is 40-60% of injection; excessive holding pressure introduces internal stress, especially PC is sensitive
Çözüm
Holding pressure set at 40-60%; thick-wall rib positions delayed; internal stress parts lower holding pressure with annealing;After adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
PC holding pressure 40-60%, balancing sink marks and stress at both ends;After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence;Include this case in the defect archive as a reference for troubleshooting similar problems in the future
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!