Menü
Malzemeler Makineler
İçgörüler
Makaleler Videolar Sorun ve Çözüm
About
Chembull Hakkında Medya Ortakları
Bize Ulaşın
Dil
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Sorun ve Çözüme Geri Dön
Processing Machinery 8 görüntüleme

DSTDP purging difficulty

Sorun Belirtisi
DSTDP purging requires 2-3h, time-consuming, affecting changeover efficiency
Neden Analizi
DSTDP adhesion strong, forming a firm adhesive layer on the screw and barrel; DSTDP thermal stability poor, becomes sticky at high temperature, harder to remove
Çözüm
1) Before purging, flush with high-viscosity PE to carry away DSTDP residue; 2) lower purging temperature below the DSTDP softening point to reduce adhesion; 3) use dedicated purging compound
Temel Çıkarım
Purging difficulty is caused by strong DSTDP adhesion; PE flushing and temperature reduction are key
DSTDPpurging difficultyadhesionPE flushingdedicated purging compound

Bu faydalı oldu mu?

0 kişi bunu faydalı buldu

ChemAI