Processing Machinery 2 views

DSTDP purging difficulty

Problem Phenomenon
DSTDP purging requires 2-3h, time-consuming, affecting changeover efficiency
Cause Analysis
DSTDP adhesion strong, forming a firm adhesive layer on the screw and barrel; DSTDP thermal stability poor, becomes sticky at high temperature, harder to remove
Solution
1) Before purging, flush with high-viscosity PE to carry away DSTDP residue; 2) lower purging temperature below the DSTDP softening point to reduce adhesion; 3) use dedicated purging compound
Key Takeaway
Purging difficulty is caused by strong DSTDP adhesion; PE flushing and temperature reduction are key
DSTDPpurging difficultyadhesionPE flushingdedicated purging compound