Menú
Materiales Maquinaria
Perspectivas
Artículos Vídeos Problema y solución
About
Acerca de Chembull Socios de medios
Contáctenos
Idioma
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Volver a Problema y solución
Processing Machinery 5 visualizaciones

DSTDP purging difficulty

Fenómeno del problema
DSTDP purging requires 2-3h, time-consuming, affecting changeover efficiency
Análisis de la causa
DSTDP adhesion strong, forming a firm adhesive layer on the screw and barrel; DSTDP thermal stability poor, becomes sticky at high temperature, harder to remove
Solución
1) Before purging, flush with high-viscosity PE to carry away DSTDP residue; 2) lower purging temperature below the DSTDP softening point to reduce adhesion; 3) use dedicated purging compound
Conclusión clave
Purging difficulty is caused by strong DSTDP adhesion; PE flushing and temperature reduction are key
DSTDPpurging difficultyadhesionPE flushingdedicated purging compound