Extrusion & Post 11 görüntüleme

Glass Fibre extrusion rough surface

Sorun Belirtisi
Glass Fibre extruded product surface roughness Ra>5μm, exceeding requirement
Neden Analizi
Extrusion temperature too low <160°C, melt flow unstable; die inner wall rough or damaged; Glass Fibre melt elasticity, extrusion swell uneven
Çözüm
1) Raise extrusion temperature to 160-220°C; 2) polish die inner wall Ra<0.4μm; 3) reduce extrusion rate 10-15%; 4) add 0.3-0.5wt% external lubricant
Temel Çıkarım
Rough surface is caused by low-temperature extrusion and die defects; raising temperature and polishing die are core countermeasures
Glass Fibre extrusionrough surfacedie polishingextrusion temperaturemelt elasticity