Extrusion & Post
9 Aufrufe
Glass Fibre extrusion rough surface
Problembeschreibung
Glass Fibre extruded product surface roughness Ra>5μm, exceeding requirement
Ursachenanalyse
Extrusion temperature too low <160°C, melt flow unstable; die inner wall rough or damaged; Glass Fibre melt elasticity, extrusion swell uneven
Lösung
1) Raise extrusion temperature to 160-220°C; 2) polish die inner wall Ra<0.4μm; 3) reduce extrusion rate 10-15%; 4) add 0.3-0.5wt% external lubricant
Wichtigste Erkenntnis
Rough surface is caused by low-temperature extrusion and die defects; raising temperature and polishing die are core countermeasures
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!