Menü
Malzemeler Makineler
İçgörüler
Makaleler Videolar Sorun ve Çözüm
About
Chembull Hakkında Medya Ortakları
Bize Ulaşın
Dil
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Sorun ve Çözüme Geri Dön
Extrusion & Post 11 görüntüleme

MP extruded pipe ovality exceeding standard

Sorun Belirtisi
MP extruded pipe ovality >1.05, exceeding the 1.02 standard requirement
Neden Analizi
pipe cooling uneven, single-side cooling; sizing sleeve design unreasonable; haul-off clamping force uneven causing pipe compression deformation
Çözüm
1) adopt annular spray cooling to ensure uniform temperature reduction; 2) optimize sizing sleeve inner diameter and taper design; 3) multi-track uniform clamping haul-off; 4) increase vacuum sizing section length to ensure full calibration
Temel Çıkarım
ovality is caused by uneven cooling and clamping; annular cooling and uniform haul-off are key
MP pipe ovality annular cooling vacuum sizing uniform haul-off

Bu faydalı oldu mu?

0 kişi bunu faydalı buldu

ChemAI