MP extruded pipe ovality exceeding standard

Fenómeno del problema
MP extruded pipe ovality >1.05, exceeding the 1.02 standard requirement
Análisis de la causa
pipe cooling uneven, single-side cooling; sizing sleeve design unreasonable; haul-off clamping force uneven causing pipe compression deformation
Solución
1) adopt annular spray cooling to ensure uniform temperature reduction; 2) optimize sizing sleeve inner diameter and taper design; 3) multi-track uniform clamping haul-off; 4) increase vacuum sizing section length to ensure full calibration
Conclusión clave
ovality is caused by uneven cooling and clamping; annular cooling and uniform haul-off are key