Injection Molding 7 görüntüleme

PPS '2079851475616104452 processing temperature control

Sorun Belirtisi
PPS processing temperature range 290-350°C is narrow; improper temperature causes degradation or poor filling.
Neden Analizi
PPS melting temperature is about 280°C and requires processing above 290°C, but above 350°C oxidative crosslinking and degradation occur.
Çözüm
Precisely control barrel temperature 290-330°C; avoid excessive temperature and residence time.
Temel Çıkarım
PPS heat-resistant plastic itself also has a limited processing temperature window.
PPSprocessing temperaturedegradationcrosslinkingtemperature control