Injection Molding 3 visualizaciones

PPS '2079851475616104452 processing temperature control

Fenómeno del problema
PPS processing temperature range 290-350°C is narrow; improper temperature causes degradation or poor filling.
Análisis de la causa
PPS melting temperature is about 280°C and requires processing above 290°C, but above 350°C oxidative crosslinking and degradation occur.
Solución
Precisely control barrel temperature 290-330°C; avoid excessive temperature and residence time.
Conclusión clave
PPS heat-resistant plastic itself also has a limited processing temperature window.
PPSprocessing temperaturedegradationcrosslinkingtemperature control