Injection Molding
2 visualizações
PPS '2079851475616104452 processing temperature control
Fenómeno do problema
PPS processing temperature range 290-350°C is narrow; improper temperature causes degradation or poor filling.
Análise das causas
PPS melting temperature is about 280°C and requires processing above 290°C, but above 350°C oxidative crosslinking and degradation occur.
Solução
Precisely control barrel temperature 290-330°C; avoid excessive temperature and residence time.
Conclusão principal
PPS heat-resistant plastic itself also has a limited processing temperature window.
Isto foi útil?
0 pessoas acharam isto útil