Residual Acetaldehyde from Improper Drying in PBT '2079851475616104452
Sorun Belirtisi
PBT products have a residual aldehyde odor after processing.
Neden Analizi
The drying temperature is too high or the time is too long, causing PBT thermal degradation; the processing temperature is too high, producing aldehyde decomposition products.
Çözüm
Control the drying temperature at 120°C, not exceeding 130°C; reduce the processing temperature; shorten the residence time.