Material Drying 8 visualizaciones

Residual Acetaldehyde from Improper Drying in PBT '2079851475616104452

Fenómeno del problema
PBT products have a residual aldehyde odor after processing.
Análisis de la causa
The drying temperature is too high or the time is too long, causing PBT thermal degradation; the processing temperature is too high, producing aldehyde decomposition products.
Solución
Control the drying temperature at 120°C, not exceeding 130°C; reduce the processing temperature; shorten the residence time.
Conclusión clave
PBT aldehyde odor affects the use experience.
PBTacetaldehydedrying temperaturedegradation