Material Drying 3 Aufrufe

Residual Acetaldehyde from Improper Drying in PBT '2079851475616104452

Problembeschreibung
PBT products have a residual aldehyde odor after processing.
Ursachenanalyse
The drying temperature is too high or the time is too long, causing PBT thermal degradation; the processing temperature is too high, producing aldehyde decomposition products.
Lösung
Control the drying temperature at 120°C, not exceeding 130°C; reduce the processing temperature; shorten the residence time.
Wichtigste Erkenntnis
PBT aldehyde odor affects the use experience.