Injection Molding 5 görüntüleme

Flow marks appearing on PET injection molded parts

Sorun Belirtisi
Wavy or snakeskin-like flow marks appear on the surface of PET products.
Neden Analizi
Melt temperature is on the low side and the flow front solidifies intermittently; injection speed is slow or unstable; cavity wall temperature is on the low side.
Çözüm
Increase melt temperature by 10-20°C; appropriately increase injection speed; mold temperature 130-150°C; optimize gate design.
Temel Çıkarım
PET flow marks are caused by an unstable melt front during filling.
PETflow markmelt frontfillingmold temperature