Molds & Tooling 5 görüntüleme

PETG mold cooling water channel design defect, local hot spots

Sorun Belirtisi
Insufficient cooling in local mold areas produces hot spots, where the product cools slowly and shrinks more.
Neden Analizi
Cooling water channels insufficient or clogged causing local insufficient cooling, water channel design unreasonable.
Çözüm
Use conformal cooling water channels; regularly clean the water channels; check temperature distribution with an infrared thermal imager.
Temel Çıkarım
PETG mold cooling uniformity is crucial to product quality.