Fenómeno del problema
Insufficient cooling in local mold areas produces hot spots, where the product cools slowly and shrinks more.
Análisis de la causa
Cooling water channels insufficient or clogged causing local insufficient cooling, water channel design unreasonable.
Solución
Use conformal cooling water channels; regularly clean the water channels; check temperature distribution with an infrared thermal imager.
Conclusión clave
PETG mold cooling uniformity is crucial to product quality.