Molds & Tooling 6 مشاهدة

POM Shrinkage Rate 1.8-3.5%

ظاهرة المشكلة
Large dimensional deviation of the part, shrinkage voids and sink marks in thick-walled areas, and inconsistent shrinkage at different wall thicknesses in the same mold
تحليل الأسباب
POM has high crystallinity; when transitioning from melt to crystalline solid, the shrinkage rate is 1.8-3.5% and shrinkage is greater at thick walls; wall thickness differences cause density differences, and thick-wall melt flowing toward thin walls aggravates non-uniformity
الحل
①Allow margin in the mold according to shrinkage rate and correct through mold trials; ②make wall thickness as uniform as possible; ③strengthen holding pressure feeding for thick-walled parts to prevent shrinkage voids; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
الخلاصة الأساسية
POM's shrinkage ranks among the highest in engineering plastics; uniform wall thickness, holding pressure compensation, and mold margin allowance are the three key elements of dimensional control; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
POM;shrinkage rate;1.8-3.5%;holding pressure;uniform wall thickness