Molds & Tooling 6 مشاهدة

PSU Notch Sensitivity and Fracture

ظاهرة المشكلة
PSU products fracture at right angles or sharp corners due to stress concentration; cracks propagate at notches during assembly and use; strength is far below expectations.
تحليل الأسباب
PSU products are quite sensitive to notches; stress concentration factors at right angles or sharp corners are high; the superposition of internal stress and notches accelerates fracture; under impact loads, notches become crack initiation points.
الحل
①Use arc transitions at right angles or sharp corners; ②Structural review to eliminate all sharp corners; ③Low-stress process to reduce initial stress; ④Notch impact testing to verify the design.
الخلاصة الأساسية
PSU notch sensitivity requires an absolute fillet principle in design; arc transition is a zero-cost strength improvement; stress management coordinates with structural design.; After confirming effectiveness, solidify the parameters and practices into the work instructions to prevent recurrence
PSU; notch; fracture; fillet; stress concentration; design