Extrusion & Post
12 مشاهدة
CEF surface dense pockmarks
ظاهرة المشكلة
Dense pockmarks of 0.1-0.3mm appear on the surface of the CEF product, affecting the appearance and coating adhesion
تحليل الأسباب
The raw material contains impurity particles >0.05%; the mold cavity surface is damaged or has corrosion pits
الحل
1) Replace with pure raw material with impurities <0.01%; 2) Repair and polish the mold cavity to Ra<0.2μm; 3) Filter the raw material to remove particles
الخلاصة الأساسية
Pockmarks are caused by raw material impurities and mold damage; pure raw materials and mold maintenance are the key