PAI insufficient post-curing, insufficient performance
ظاهرة المشكلة
Without post-curing, the PAI heat deflection temperature and strength are far lower than expected
تحليل الأسباب
The imidization reaction of PAI is not completed during molding; the post-curing temperature or time is insufficient
الحل
Post-cure according to the 260°C specification with stepwise heating and curing, up to 260°C and hold for a sufficient time
الخلاصة الأساسية
Post-curing is the decisive step for achieving PAI performance