Blow Molding 10 Aufrufe

HDPE '2079851475616104457 parison die lines (Die Lines)

Problembeschreibung
Longitudinal line marks on the parison surface, still visible after '2079851475616104457.
Ursachenanalyse
Foreign matter or degraded material caught between the die and mandrel; die damage and carbonized buildup also cause streaks.
Lösung
①Clean the die of foreign matter and buildup; ②check the die for damage and polish; ③increase resin temperature and back pressure to improve plasticization; ④check raw material contamination.
Wichtigste Erkenntnis
For parison line marks, clean the die first, then check the material.
HDPE; '2079851475616104457; die lines; die; buildup