Extrusion & Post
2 Aufrufe
LDPE Film Slip Agent Blooming
Problembeschreibung
White powdery precipitation appears on the film surface after storage.
Ursachenanalyse
Slip agent/antiblock agent is over-added, exceeding the compatibility limit and precipitating to the surface; affecting printing and lamination.
Lösung
①Reduce additive addition amount; ②switch to slow-migrating polymeric additives; ③control storage temperature; ④clean and evaluate precipitated film before use.
Wichtigste Erkenntnis
Blooming = excessive additive precipitation.
War das hilfreich?
0 Personen fanden dies hilfreich