Extrusion & Post
7 visualizações
LDPE Film Slip Agent Blooming
Fenómeno do problema
White powdery precipitation appears on the film surface after storage.
Análise das causas
Slip agent/antiblock agent is over-added, exceeding the compatibility limit and precipitating to the surface; affecting printing and lamination.
Solução
①Reduce additive addition amount; ②switch to slow-migrating polymeric additives; ③control storage temperature; ④clean and evaluate precipitated film before use.
Conclusão principal
Blooming = excessive additive precipitation.
Isto foi útil?
0 pessoas acharam isto útil