Extrusion & Post 3 visualizaciones

LDPE Film Slip Agent Blooming

Fenómeno del problema
White powdery precipitation appears on the film surface after storage.
Análisis de la causa
Slip agent/antiblock agent is over-added, exceeding the compatibility limit and precipitating to the surface; affecting printing and lamination.
Solución
①Reduce additive addition amount; ②switch to slow-migrating polymeric additives; ③control storage temperature; ④clean and evaluate precipitated film before use.
Conclusión clave
Blooming = excessive additive precipitation.
LDPE; film; blooming; slip agent; precipitation