Extrusion & Post 11 Aufrufe

EAA surface snakeskin texture

Problembeschreibung
Snakeskin-like irregular texture on the surface of EAA extruded products
Ursachenanalyse
Extrusion temperature too low, uneven melt elastic recovery; uneven die temperature distribution
Lösung
1) Increase extrusion temperature to the processing temperature range; 2) Homogenize die temperature to ±2°C; 3) Reduce extrusion rate to reduce elastic recovery
Wichtigste Erkenntnis
Snakeskin texture is caused by low-temperature extrusion and elastic recovery; raising temperature and reducing speed is key
EAAsnakeskin textureextrusion temperatureelastic recoverydie temperature control